Lot weight (approx 145 pies) ............ 70 kg
Add water @ L : R = 1 : 8 .............. 560 Liters
Add Acetic Acid @ 0.6 gm / liter ............ 336gm
Cationic Softener @ 1 gm / liter.............. 560 gm
Silicon (ME) @ 0.5 gm / liter ................ 280 gm
Temperature.......................... 40°c
Time................................ 15 to 20 minutes
Drain the bath